STABILITY OF PARATHION ON ATTAPULGITE AS AFFECTED BY STRUCTURAL AND HYDRATION CHANGES
Attapulgite Dehydration Infrared spectroscopy Isomerization Parathion Scanning electron microscopy Thermal treatment
2011/11/15
Abstract--The structure and hydration status of attapulgite clay after heating at elevated temperatures and the stability of parathion on these clays was studied. Using infrared spectroscopy and scann...
Surface Reactions of Parathion on Clays
Adsorption Catalysis Hydrolysis Insecticide Parathion
2011/11/22
Abstract: The adsorption-catalyzed degradation of parathion on clay surfaces is a hydrolysis process, proceeding either directly or through a rearrangement step. The rate and mechanism of degradation ...